Pink Aluminum Oxide Is Sharp And Angular Used In Tool Grinding, Sharpening

Pink Fused Alumina is produced by doping Chromia into Alumina, which gives the material pink color. The incorporation of the Cr2O3 into the Al2O3 crystal lattice produces a slight increase in toughness and a reduced friability compared with White Fused Alumina. Compared to Brown Regular Aluminum Oxide the Pink material is harder, more aggressive and has better cutting ability. The grain shape of Pink Aluminum Oxide is sharp and angular.

Products Details

Pink Fused Alumina is produced by doping Chromia into Alumina, which gives the material pink color. The incorporation of the Cr2O3 into the Al2O3 crystal lattice produces a slight increase in toughness and a reduced friability compared with White Fused Alumina. Compared to Brown Regular Aluminum Oxide the Pink material is harder, more aggressive and has better cutting ability. The grain shape of Pink Aluminum Oxide is sharp and angular.The FEPA F grades are especially suitable for the manufacturing vitrified bonded abrasives for working hardened steels and alloys with tensile strengths of over 50 kg/mm². It is also used in tool grinding, knife-sharpening applications, precision grinding, profile grinding, flute grinding, tooth grinding, dry grinding of blade segments and mounted wheels.The FEPA P grades are a preferred material for working non-ferrous metals and
Items/ Chemical  Composition

Unit

Medium Chrome Low Chrome High Chrome
Size: F12-F80 Al2O3 % 98.2min 98.5min 97.4min
Cr2O3 % 0.45-1.00 0.20-0.45 1.00-2.00
Na2O % 0.55max 0.50max 0.55max
F90-F150 Al2O3 % 98.20min 98.50min 97.00min
Cr2O3 % 0.45-1.00 0.20-0.45 1.00-2.00
Na2O % 0.60max 0.50max 0.60max
F180-F220 Al2O3 % 97.80min 98.00min 96.50min
Cr2O3 % 0.45-1.00 0.20-0.45 1.00-2.00
Na2O % 0.70max 0.60max 0.70max
Physical Property Basic Minerals α— AI2O3 α— AI2O3 α— AI2O3
Crystal size μm 600~2000 600~2000 600~2000
True density g/cm3 ≥3.90 ≥3.90 ≥3.90
Bulk density g/cm3 1.40~1.91 1.40~1.91 1.40~1.91
Knoop hardness g/mm2 2200~2300 2200~2300 2200~2300
Application 1. Pink fused alumina for surface processing: metal oxide layer, carbide black skin, metal or non-metal surface rust removal, such as gravity die-casting mold, rubber mold oxide or free agent removal, ceramic surface black spot, uranium removal, painted rebirth. 2. Pink fused alumina beautification processing: all kinds of gold, gold jewelry, precious metal products of the extinction or fog surface processing, crystal, glass, ripple, acrylic and other non-metallic fog surface processing and can make the surface of the processing into metallic luster. 3. Pink fused alumina for Etching and processing: etching artists of jade, crystal, agate, semi-precious stone, seal, elegant stone, antique, marble tombstone, ceramics, wood, bamboo, etc. 4. Pink fused alumina for Pretreatment: TEFLON, PU, rubber, plastic coating, rubber ROLLER, electroplating, metal spray welding, titanium plating and other pretreatment, so as to increase the surface adhesion. 5. Pink fused alumina for Burr processing: burr removal of bakelite, plastic, zinc, aluminum die-casting products, electronic parts, magnetic cores, etc. 6. Pink fused alumina for stress elimination processing: aerospace, national defense, precision industry parts, rust removal, painting, polishing, such as stress elimination processing.